Open the wick size guide →A tunneling candle burns straight down the middle and leaves a thick wall of unused wax around the edge. It wastes wax, shortens burn time, and can drown the wick. The good news is that tunneling has a few clear causes, and most of them are easy to fix.
What tunneling looks like
After a few burns you see a narrow hole around the wick, while the outer wax stays solid. Over time the hole gets deeper, the flame sinks, and the scent throw weakens because only a small pool of wax is melting.
Cause 1: the first burn was too short
Wax has a kind of “memory”. On the first burn, the melt pool sets a boundary. If the candle is blown out before the melt pool reaches the edge of the container, later burns tend to stop at the same ring.
Rule of thumb: on the first burn, let the candle burn about one hour for every inch of container diameter. A 3 inch jar needs about 3 hours. Our Wick Size Guide shows this time for your container.
Cause 2: the wick is too small
If the wick cannot produce enough heat, the melt pool never reaches the wall, no matter how long the candle burns. Signs of an undersized wick:
- The melt pool is still narrow after 3 to 4 hours.
- The flame is small and weak.
- The melt pool is shallow (under about 1/4 inch deep).
The fix is a larger wick, or two wicks for wide containers. As a general guide, containers wider than about 3.5 inches usually need two wicks. Read how to tell if a wick is too big or too small.
Cause 3: short burn sessions
Even a well-made candle can tunnel if it is always burned for 30 minutes at a time. Each short burn makes the tunnel a little deeper. This is worth printing on your candle labels: “Burn until the wax melts to the edge, usually 2 to 4 hours.”
How to fix a candle that is already tunneling
The foil collar method
- Wrap a band of aluminum foil around the top of the jar so it covers the outer wax and leaves an opening of about an inch in the middle.
- Light the candle and let it burn. The foil reflects heat onto the outer wax.
- After an hour or two, check that the wax has melted level to the edge. Remove the foil carefully; it will be hot.
The heat gun method
Use a heat gun or hair dryer on low to melt the top layer of wax until it is level, then let it cool. This also works well for rough tops on new candles. Keep the heat moving and never point it at a lit candle.
Pour out excess wax
If the tunnel is so deep that the wick is drowning, blow out the candle, carefully pour off some of the liquid wax, and relight once the wick is free.
How to prevent tunneling in the candles you make
| What to check | Why it matters |
|---|---|
| Wick size and number of wicks | The flame must melt the full diameter |
| Inside diameter of the container | Wider jars need more heat |
| Wax type | Soy and coconut often need a slightly larger wick than paraffin |
| Fragrance load | Very high loads can affect how the wick burns |
| Burn instructions on the label | Customers need to know the first burn rule |
The best prevention is a proper burn test before you sell a design. Burn a test candle for 3 to 4 hours and check that the melt pool reaches the edge evenly.
Quick summary
- First burn: about one hour per inch of diameter.
- Small, weak flame and narrow pool: size up the wick.
- Wide jar: consider two wicks.
- Rescue with a foil collar or a heat gun.
- Always burn test new designs.